1204 |
SEM picture of erosion corrosion rippling patterns on steel 15Mo3, downstream a weld bead (magnification: x 100), Right: cross section of the sample. (foto KEMA ref 28 and 60). |
|
|
|
|
|
|
|
|
|
|
1205 |
Erosion-corrosion rippling of heat-loaded (A and C) and non heat-loaded (B and D) specimens from 14Mn4 steel. Magnifications x 100. (foto KEMA ref 28) |
|
|
|
|
|
|
|
|
|
|
1206 |
Rippling pattern in 14Mn4 (1D6). A: sample from cased tube (magnification x 100). B:
sample from inside cased area. Deposition rippling in A (cased area) and erosion-corrosion rippling in
B (outside cases=d area). (foto KEMA ref 28) |
|
|
|